Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.70 J/cm²

@Temperature -20.0 °C
36.6 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Daplen™ EE340AE Polypropylene TPO Compound
Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..