Polymer Property : Charpy Impact Unnotched = 37.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.90 J/cm²

@Temperature -30.0 °C
37.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber
SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme..
Charpy Impact Unnotched 7.90 J/cm²

@Temperature 23.0 °C
37.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli..