Polymer Property : Charpy Impact Unnotched = 40.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.40 J/cm²

@Temperature -30.0 °C
40.0 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 8.40 J/cm²

@Temperature 23.0 °C
40.0 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber
PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic..
Charpy Impact Unnotched 8.40 J/cm²

@Temperature -30.0 °C
40.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber
SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers
Charpy Impact Unnotched 8.40 J/cm²

@Temperature -30.0 °C
40.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled
Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime..
Charpy Impact Unnotched 8.40 J/cm²

@Temperature 23.0 °C
40.0 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
DSM Novamid® 3021GH30 NAT PA66-GF30
30% Glass Reinforced, Heat Stabilized
Charpy Impact Unnotched 8.40 J/cm²

@Temperature 23.0 °C
40.0 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
DSM Novamid® 3021GH30 BK629 PA66-GF30
30% Glass Reinforced, Heat Stabilized
Charpy Impact Unnotched 8.40 J/cm²

@Temperature 23.0 °C
40.0 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
Zytel® 70G35HSRX BK099 a 35% glass reinforced, heat stabilized, hydrolysis resistant PA66 for injection molding. Developed for applications designed for direct overmolding of gaskets onto thermopla..