Polymer Property : Charpy Impact Unnotched = 40.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.60 J/cm²

@Temperature -30.0 °C
40.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber
SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char..
Charpy Impact Unnotched 8.60 J/cm²

@Temperature 23.0 °C
40.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled
Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime..