Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 9.90 J/cm²

@Temperature 23.0 °C
47.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry)
Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS ..