Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 BT LS PA66, basic type FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. UV stabile. Used in automotive, electrical, engine.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 BT Polyamide 66 FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at low temperatures. Use in automotive, electrical, engineering and cons.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S RV500 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G8U (Dry) 43% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers PA 66, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® KU 2-7003 000000 PBT PBT, non-reinforced, injection molding |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eU |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® B 2505 000000 PBT PBT, non-reinforced, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Terluran® HH-106 Q109 Colored ABS Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXLAC 340Q Acrylonitrile Butadiene Styrene Saxalac 340Q is an siliconized, UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tes.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-HG6 (Cond.) 30% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-HG6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide A28 PA66, Injection Molding Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature 23.0 °C |
>= 47.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide B28 PA6, Injection Molded Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature 23.0 °C |
>= 47.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | >= 10.0 J/cm² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 10.0 J/cm² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K-FHG0 (Cond.) 50% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |