Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 12.3 J/cm² @Temperature 23.0 °C |
58.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 3010N 5-SL4-3X NAT PA66 FR Low Viscosity, Molding Release, 30% Glass Reinforced |