Polymer Property : Notched Tensile Strength = 2068 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Notched Tensile Strength 2068 MPa
299900 psi
Latrobe Lescalloy® Jethete M-152 ESR 1.5" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Notched Tensile Strength 2068 - 2227 MPa
299900 - 323000 psi
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Notched Tensile Strength 2068 MPa
299900 psi
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..