Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 1.4715 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.4715 MPa

@Temperature 1400 °C,
Time 10800 sec
213.42 psi

@Temperature 2550 °F,
Time 3.00 hour
Chosun Refractories BM-2 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.4715 MPa

@Temperature 1000 °C,
Time 10800 sec
213.42 psi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSM-34 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.4715 MPa

@Temperature 1000 °C,
Time 10800 sec
213.42 psi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories ZM-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.4715 MPa

@Temperature 1000 °C,
Time 10800 sec
213.42 psi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories BM-1 Air-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Adhesive Bond Strength 1.4715 MPa

@Temperature 1000 °C,
Time 10800 sec
213.42 psi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories ZM-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved