Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 10.0 MPa @Temperature 121 °C |
1450 psi @Temperature 250 °F |
Lap Shear |
Henkel Hysol AL 2000 Primer Heat-curing, nitrile phenolic, water-based primer. Cured product furnishes excellent resistance to chemicals and water. Qualified to Boeing BMS 5-42, Type 3.Applications: Sprayable Low Viscosity We.. |