Mechanical Properties Metric English Comments
Adhesive Bond Strength 11.7 MPa

@Temperature 93.0 °C
1700 psi

@Temperature 199 °F
Tensile Lap Shear
Henkel Hysol EA 9321 Paste Adhesive System
Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair