Polymer Property : Adhesive Bond Strength = 16.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 16.5 MPa

@Temperature 177 °C
2390 psi

@Temperature 351 °F
Lap Shear
Henkel Hysol PL 737 Film Adhesive
Nonmetallic, modified epoxy film specifically designed for use in structural aircraft components. Low flow characteristics.Application: Metal and Honeycomb Bonding
Adhesive Bond Strength 16.5 MPa

@Temperature 23.9 °C
2390 psi

@Temperature 75.0 °F
on aluminum; ASTM D1002-64
3M Pronto™ CA-7 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting product with ..