Mechanical Properties Metric English Comments
Adhesive Bond Strength 11.6 MPa

@Temperature 25.0 °C
1680 psi

@Temperature 77.0 °F
tube shears
Henkel Hysol PL 460 Core Splice Adhesive
Foaming epoxy adhesive in paste form for easy extrusion through packaged cartridges. Expands and cures at temperatures from 250°F / 121°C to 350°F / 177°C. Qualified to Boeing BMS 5-90, Type IV...