Polymer Property : Adhesive Bond Strength = 24.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 24.0 MPa

@Temperature -55.0 °C
3480 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 9394/C-2 Paste Adhesive System
Elevated cure, thixotropic adhesive with structural properties to 450°F / 232°C.Application: Structural Repair