Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 26.9 MPa @Temperature 25.0 °C |
3900 psi @Temperature 77.0 °F |
Lap Shear |
Henkel Hysol PL 795 Film Adhesive Epoxy film adhesive designed for composite bonding applications. May cure at 250°F / 121°C or 350°F / 177°C, with service temperatures up to 350°F / 177°C. Ideal for co-cure or secondary bondi.. |