Mechanical Properties Metric English Comments
Adhesive Bond Strength 22.8 MPa

@Temperature -55.0 °C
3310 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 9394 Paste Adhesive System
Thixotropic adhesive with structural properties to 350°F / 177°C.Applications: Potting Structural Repair Composite Bonding Liquid Shim
Adhesive Bond Strength 22.8 MPa

@Temperature -55.0 °C
3310 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 9396 Paste Adhesive System
Two-part, low viscosity, unfilled version of Hysol EA 9394. Qualified to BMS 8-301.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding