Mechanical Properties Metric English Comments
Adhesive Bond Strength 4.10 MPa

@Temperature 23.9 °C
595 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-100 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Toughened material that provide..