Polymer Property : Adhesive Bond Strength = 6.20 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-7 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting product with ..
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-9 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A slower setting version of CA-..
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-4 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Fast setting multi-purpose cyan..
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-40 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting adhesive with..
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-40H Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A higher viscosity, slower sett..
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-5 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high viscosity, slower settin..
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on aluminum; ASTM D1002-64
3M Pronto™ CA-50 Gel Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high-viscosity gel consistenc..
Adhesive Bond Strength 6.20 MPa

@Temperature 23.9 °C
899 psi

@Temperature 75.0 °F
on ABS; ASTM D1002-64
3M Pronto™ CA-8 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Fast setting adhesive with exce..