Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.00 MPa

@Temperature 121 °C
1160 psi

@Temperature 250 °F
tube shears
Henkel Hysol MA 562 Core Splice Adhesive
General-purpose 250°F / 121°C or 350°F / 177°C curing foaming adhesive. Designed for service temperatures from -67°F / -55°C to 350°F / 177°C. Medium tack, nonmetallic, low exotherm properti..