Izod Impact, Unnotched (ISO) 102 kJ/m²
48.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RV00CE PA 66 (Europe-Africa-Middle East)
LNP VERTON* RV00CE is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 102 kJ/m²
48.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific)
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 102 kJ/m²
48.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RV00CES PA 66
LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Izod Impact, Unnotched (ISO) 102 kJ/m²
48.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Izod Impact, Unnotched (ISO) 102 kJ/m²
48.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific)
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 102 kJ/m²
48.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON RX06424 PA 66
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural