Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 1029 kJ/m²
489.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer
LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 1029 kJ/m²
489.6 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.