Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 217 kJ/m²
103 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC
LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant.