Izod Impact, Unnotched (ISO) 27.6 kJ/m²

@Temperature 0.000 °C,
Time 86400 sec
13.1 ft-lb/in²

@Temperature 32.0 °F,
Time 24.0 hour
Shandong Rike Chemical HELIâ„¢ HL-708A Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..