Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 165 kJ/m² | 78.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DI001E PC (Europe-Africa-Middle East) LNP* Lubricomp* DI001E is a compound based on Polycarbonate resin containing Silicone. Added features include: Internally Lubricated, Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 165 kJ/m² | 78.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA 11 (Asia Pacific) LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing Glass Bead. |
|||
Izod Impact, Unnotched (ISO) | 165 kJ/m² | 78.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11 LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead. |