Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 181 kJ/m²

@Temperature -30.0 °C
86.1 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm
Izod Impact, Unnotched (ISO) 181 kJ/m²
86.1 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific)
Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame..
Izod Impact, Unnotched (ISO) 181 kJ/m²

@Temperature -40.0 °C
86.1 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman 9921P PET Film  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Izod Impact, Unnotched (ISO) 181 kJ/m²
86.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC
LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding.