Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral filled PA6 non-halogen FR compound
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP CX05031 PS (Europe-Africa-Middle East)
LNP* Lubricomp* CX05031 is a compound based on Polystyrene resin containing Graphite, Silicone. Added features include; Internally Lubricated.
Izod Impact, Unnotched (ISO) 5.00 - 10.0 kJ/m²
2.38 - 4.76 ft-lb/in²
Average value: 7.57 kJ/m² Grade Count:10
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Unnotched (ISO) >= 5.00 kJ/m²
>= 2.38 ft-lb/in²
ISO 180/1A
Iran Petrochemical (PCC) Tabriz 6630/1 High Impact Polystyrene  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming.
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East)
50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant.
Izod Impact, Unnotched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp FX05032 PE (Europe-Africa-Middle East)
LNP* THERMOCOMP* FX05032 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added features include : Foaming Agent for Polyolefins.This data was supplied by SABIC-IP for t..
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP WX93111 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WX93111 is a compound based on Polybutylene Terephalate resin containing Flame retardant , Glass Fiber, Proprietary filler. Added features include : Improved CTI.
Izod Impact, Unnotched (ISO) 5.00 kJ/m²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
DSM Arnitel® PL650 Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starglas FX05032 PE
Starglas FX05032 is Polyethylene Resin with a Proprietary Additive (foaming agent for polyolefins)Information provided by Eurostar.
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
Axion Polymers Axplas® PS04 0000 Mixed Polystyrene Granules with FR
The PS04 series of clean, mixed polystyrene granular chips offers a low-cost option for manufacturers to add post-consumer, engineering polymers to a wide range of products. The polymer mix includes..
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180/1U
A.D. Compound Adene NCWA Homopolymer 60% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
Axion Polymers Axplas® PS07 0000 General Purpose Polystyrene