Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 5.30 - 18.2 kJ/m²
2.52 - 8.66 ft-lb/in²
ISO R179
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound