Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 39.0 - 47.0 kJ/m² @Temperature -30.0 - -30.0 °C |
18.6 - 22.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 42.7 kJ/m² Grade Count:5 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |