Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 24.2 - 34.7 kJ/m² | 11.5 - 16.5 ft-lb/in² | Average value: 28.4 kJ/m² Grade Count:4 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched (ISO) | 24.2 kJ/m² | 11.5 ft-lb/in² | ISO 180 |
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Izod Impact, Unnotched (ISO) | 24.2 - 31.0 kJ/m² | 11.5 - 14.8 ft-lb/in² | Average value: 27.8 kJ/m² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Izod Impact, Unnotched (ISO) | 24.2 kJ/m² | 11.5 ft-lb/in² | ISO 180 |
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |