Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC
LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC (Asia Pacific)
LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper..
Izod Impact, Unnotched (ISO) 68.0 kJ/m²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HFD4271 PC
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
Izod Impact, Unnotched (ISO) 68.0 kJ/m²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
Izod Impact, Unnotched (ISO) 68.0 kJ/m²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp JL003 PES
LNP* Lubricomp* JL003 is a compound based on Polyethersulfone resin containing PTFE.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized...
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 (Asia Pacific)
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
Type 1; ISO 180
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree..
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
ISO 180
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface ..
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX04462C PC
LNP STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
GB/T 1843-2008
Sichuan Deyang Haton® hGR505 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66
LNP* THERMOCOMP* RC006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66
LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX04462C PC (Asia Pacific)
LNP* STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10
LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 (Asia Pacific)
LNP* Thermocomp* RC006 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66
LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON PX91200 PA 6
LNP VERTON* PX91200 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: High Impact, Structural
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Star L PA6 D61 PA6, Injection Molded
Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 68.0 kJ/m²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..