Polymer Property : Izod Impact, Unnotched (ISO) = 4.04 ft-lb/in²
Polymer Property :
Izod Impact, Unnotched (ISO) =
4.04 ft-lb/in²
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Unnotched (ISO)
8.50
kJ/m²
4.04
ft-lb/in²
ISO 180/1U
A.D. Compound Adene NTWA Homopolymer 60% Talc Filled Polypropylene