Polymer Property : Izod Impact, Unnotched (ISO) = 41.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 87.8 kJ/m²
41.8 ft-lb/in²
ISO 180
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..