Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | >= 5.40 kJ/m² | >= 2.57 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.3 |
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical applications (coarse weave: >130 g/m2, =30 threads/cm). Better mechanical properties and poorer electrical properties than type PF CC 202.Information provided by Hippe. |