Polymer Property : Izod Impact, Unnotched (ISO) = 54.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 115 kJ/m²
54.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66
LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant.
Izod Impact, Unnotched (ISO) 115 kJ/m²
54.7 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starflam PX06012 PA6, Flame Retardant, Injection Molded
Starflam PX06012 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.