Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 120 kJ/m²
57.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East)
LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color
Izod Impact, Unnotched (ISO) 120 kJ/m²
57.1 ft-lb/in²
ISO 180
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Izod Impact, Unnotched (ISO) 120 kJ/m²

@Temperature 23.0 °C
57.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon DD0009XQ PC (Europe-Africa-Middle East)
LNP* Stat-Kon* DD0009XQ is a compound based on Polycarbonate containing Carbon Powder and Flame Retardant. Added features include Electrically Conductive, Flame Retardant and Easy Molding.This data..
Izod Impact, Unnotched (ISO) 120 kJ/m²
57.1 ft-lb/in²
Shandong Guangyin 1212 Reinforced Nylon
Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cab..
Izod Impact, Unnotched (ISO) 120 kJ/m²
57.1 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Star L POM D11 POM, Injection Molded
Star L POM D11 is Silicone Oil Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.