Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 0.700 - 7.00 kJ/m²

@Temperature -40.0 - -30.0 °C
0.333 - 3.33 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.58 kJ/m² Grade Count:12
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Izod Impact, Notched (ISO) 0.700 kJ/m²

@Temperature 23.0 °C
0.333 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..