Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.20 kJ/m² - NB @Temperature -20.0 - -20.0 °C |
0.571 ft-lb/in² - NB @Temperature -4.00 - -4.00 °F |
Average value: 5.84 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched (ISO) | 1.20 kJ/m² - NB @Thickness 4.00 - 4.00 mm |
0.571 ft-lb/in² - NB @Thickness 0.157 - 0.157 in |
Average value: 5.84 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |