Polymer Property : Izod Impact, Notched (ISO) = 1.33 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.80 - 45.0 kJ/m²
1.33 - 21.4 ft-lb/in²
Average value: 10.6 kJ/m² Grade Count:8
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Izod Impact, Notched (ISO) 2.80 kJ/m²
1.33 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CRG800 Acrylic Polymer, Toughened Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Izod Impact, Notched (ISO) 2.80 kJ/m²
1.33 ft-lb/in²
80x10x4; ISO 180/1A
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded
Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar.
Izod Impact, Notched (ISO) 2.80 kJ/m²
1.33 ft-lb/in²
ISO 180/1A
A.D. Compound Adene NCQA Homopolymer 40% CaCO3 Filled Polypropylene
Information provided by A.D. Compound