Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 10.2 kJ/m² | 4.85 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hMR61LC1 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |