Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 25.3 kJ/m²
12.0 ft-lb/in²
ISO 180
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..