Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 14.1 kJ/m² | 6.70 ft-lb/in² | Area; ASTM D256 |
ExxonMobil HDPE HYA 600 High Density Polyethylene Resin Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & M.. |
|||
Izod Impact, Notched (ISO) | 14.1 kJ/m² | 6.71 ft-lb/in² | ISO 180 |
LNP Thermocomp® IF-1006 Polyamide 6/12 Copolymer, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |