Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS Cycoloy Medium Heat Plating Grade for Automotive |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ASTM D256 |
Lushan PJ-1 Polypropylene Compounds for Steel Pipe Top Coats Polypropylene compound for steel pipe top coats Lushan PJ-1 is used for 3LPP coating system in colored white. It is supplied in pellets for melt extrusion or in a powder for application by spray or .. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East) Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | ISO 180 |
Styrolution Styrolux® 3G46 SBC Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -10.0 °C |
14.3 ft-lb/in² @Temperature 14.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON WV006 PBT (Europe-Africa-Middle East) LNP VERTON* WV006 is a compound based on Polybutylene Terephalate resin containing Long Glass. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® FR3040 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -50.0 °C |
14.3 ft-lb/in² @Temperature -58.0 °F |
|
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific) Cycoloy Medium Heat Plating Grade for Automotive |
|||
Izod Impact, Notched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |