Polymer Property : Izod Impact, Notched (ISO) = 14.5 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 14.5 kJ/m²
6.90 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Izod Impact, Notched (ISO) 14.5 kJ/m²
6.90 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® C 402 M PA6, DRY
Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high ..
Izod Impact, Notched (ISO) 14.5 kJ/m²

@Temperature 23.0 °C
6.90 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DSM Akulon® M-1016 (Dry) 33% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Izod Impact, Notched (ISO) 14.5 kJ/m²

@Temperature 23.0 °C
6.90 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned)
Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF
Izod Impact, Notched (ISO) 14.5 kJ/m²

@Temperature 23.0 °C
6.90 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® A3WG10 BK 00564 50% Glass Filled PA66 (Conditioned)
Description: 50% glass-fiber reinforced injection-molding grade with high heat aging resistance for technical articles of very high stiffness.Information provided by BASF