Polymer Property : Izod Impact, Notched (ISO) = 142 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 142 kJ/m²
67.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC
LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated.