Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.04 kJ/m² | 2.40 ft-lb/in² | ASTM D256 |
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66 Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan.. |
|||
Izod Impact, Notched (ISO) | 5.04 kJ/m² | 2.40 ft-lb/in² | ASTM D256 |
Nilit Polynil® P60 Medium Viscosity Nylon 66 Description: Polynil P60 is a grade has a viscosity that has been optimized for monofilament extrusion.Key characteristics: Viscosity number 155 gr/cm3Excellent melt stabilityHigh elongationInformat.. |
|||
Izod Impact, Notched (ISO) | 5.04 kJ/m² | 2.40 ft-lb/in² | ISO 180/1A |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |