Polymer Property : Izod Impact, Notched (ISO) = 20.9 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 20.9 kJ/m²
9.95 ft-lb/in²
ISO 180
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **
Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..