Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 44.1 kJ/m² | 21.0 ft-lb/in² | ASTM D256 |
GEHR Plastics ECOGEHR® PA 6.10 Nylon 6.10 Dry, 60% Sebacic Acid Nylon 6.10 is 60 % sebacic acid, which is obtained from castor oil. This material combines a low density (for polyamide) with good cold impact strength, and its low water absorption makes it very di.. |