Izod Impact, Notched (ISO) 51.0 kJ/m²
24.3 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS
PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact
Izod Impact, Notched (ISO) 51.0 kJ/m²
24.3 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® RCY6214 PC+ABS (Asia Pacific)
Cycoloy* RCY6214 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.5 mm. D..
Izod Impact, Notched (ISO) 51.0 kJ/m²

@Temperature 0.000 °C
24.3 ft-lb/in²

@Temperature 32.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific)
Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5..
Izod Impact, Notched (ISO) 51.0 kJ/m²
24.3 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ADX1016R PC (Europe-Africa-Middle East)
Lexan Copolymer resin with improved chemical resistance, available only in limited colors.
Izod Impact, Notched (ISO) 51.0 kJ/m²
24.3 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific)
Designed for outdoor telecommunications enclosure applications.
Izod Impact, Notched (ISO) 51.0 kJ/m²

@Temperature -30.0 °C
24.3 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific)
PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability
Izod Impact, Notched (ISO) 51.0 kJ/m²

@Temperature -30.0 °C
24.3 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
Izod Impact, Notched (ISO) 51.0 kJ/m²
24.3 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific)
FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.