Izod Impact, Notched (ISO) 24.6 kJ/m²
11.7 ft-lb/in²
ASTM D256
GEHR Plastics ECOGEHR® C-L Cellulose-Lignin Compound  (discontinued **)
C-L is comprised of the wood components cellulose, natural fibers, lignin and fatty acids. It possesses many interesting properties that together are very similar to the natural wood. Consequently,..