Polymer Property : Izod Impact, Notched (ISO) = 29.4 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 29.4 kJ/m²

@Temperature -50.0 °C
14.0 ft-lb/in²

@Temperature -58.0 °F
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili..